I'm doin a project to produce silver impregenated activated carbon.finish the production in 50 minutes but now it takes 3hours which is a loss.
This is the whole thing!
We put 6 canisters inside the chaimber filled with activated carbon and inside of it we mix silver nitrate solution(40% of the weight of the carbon) and mix it before heating it.We have 6 L.P gas burners inside the chaimber and we want to heat it for 450 degrees.We were planning to get rid of the steam within 20 minutes(practically it takes 2 hours) .So i need to find a method to increase the heat transfer rate inside the chaimber and maintain a steady temperature of 450degrees.
If we could get rid of the steam from 6 canisters(length of a canister is 700mm) within 30 minutes we are done.But how? know only 2 methods
1.By drying the mixture outside and do the pyrolysis process inside the chaimber.
2.finding a method to transfer heat uniformly inside the canister
wt douthink?
2007-01-25
17:31:00
·
1 answers
·
asked by
SOAD_ROX
2
in
Science & Mathematics
➔ Engineering
Ed ur answer is really sensible and it hits the point.But the problem is if i change the AgNO3 solution everything will change.Coz AgNO3 solution is made in the most precise maner so i cant change it.
I agree with the vacuum thing.Thats a good idea.
If u get to know any other methods please do mail me.My email address is