English Deutsch Français Italiano Español Português 繁體中文 Bahasa Indonesia Tiếng Việt ภาษาไทย
All categories

I made my own flowers, leaves, hearts etc to embellish my stepping stones. I used a low fire glaze and low fire clay. After winter months were over I noticed the glaze chipping off. Any sugguestions?? TIA Jane

2007-06-14 09:22:02 · 2 answers · asked by Jane H 1 in Home & Garden Garden & Landscape

2 answers

yea, it's breaking off for the same reason clay pots break. It's caused by freezing water in the porous surfaces during winter. The expansion of the freezing water cracks and separates the glaze from the clay. Next time try a high fire clay and glaze.

2007-06-14 09:30:09 · answer #1 · answered by Sptfyr 7 · 0 0

Yes get better paint dumb ***!!!

2007-06-14 09:26:50 · answer #2 · answered by Jones 1 · 0 0